Numéro
J. Phys. IV France
Volume 06, Numéro C8, Décembre 1996
ICIFUAS 11
Eleventh International Conference on Internal Friction and Ultrasonic Attenuation in Solids
Page(s) C8-699 - C8-702
DOI https://doi.org/10.1051/jp4:19968152
ICIFUAS 11
Eleventh International Conference on Internal Friction and Ultrasonic Attenuation in Solids

J. Phys. IV France 06 (1996) C8-699-C8-702

DOI: 10.1051/jp4:19968152

Dielectric Relaxation Measurements in the Protonic Conductors SrCeO3 and SrZrO3

L. Zimmermann, S. Bausch, H.G. Bohn and W. Schilling

Institut für Festkörperforschung, Forschungszentrum Jülich GmbH, 52425 Jülich, Germany


Abstract
Dielectric relaxation spectroscopy has been applied to the protonic conductors SrCe0.95Yb0.05O3-α and SrZr0.95Y0.05O3-α. In both systems two different types of relaxation peaks were observed which are characteristic of the wet (proton containing) and dry (proton free) state of the samples. They correspond to peaks found by mechanical relaxation. This shows that the defects underlying the relaxation mechanism possess both an electric and an elastic dipole moment thus giving rise to both dielectric and mechanical relaxation.



© EDP Sciences 1996