Giant magneto-impedance in glass covered microwires
J.P. Sinnecker, E.H.C.P. Sinnecker, A. Zhukov, J.M. Garcia-Beneytez, M.J. Garcia Prieto and M. VázquezInstituto de Magnetismo Aplicado, Apartado de Correos 155, 28230 Las Rozas, Madrid, Spain
Abstract
Giant magneto-impedance ratio in glass covered Co68.5Mn6.5Si10B15 microwires, with different glass coat thickness, was measured as a function of de axial field (up to 10.5 kA/m) and frequency (f=0.5 MHz up to 30 MHz). A maximum GMI ratio of 58% was observed at 1.5 MHz. The frequency dependence of the GMI maximum and the position where it occurs is discussed in terms of the glass coat thickness.